Physical Properties of 439 Alloys in the Annealed Condition at -20°F to +100°F

      Tensile Strength Yield Strength            
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion IN./ IN./ °F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
439 S43035 A268 60,000 (415) 60 30,000 (205) 30 20 90 Rb 29.0 5.6 168

Composition of 439 tubing and pipe

Grade 439
UNS Designation S43035
Nickel (Ni) 0.50
Chromium (Cr) 17.0 – 19.0
Iron (Fe) Bal.
Molybdenum (Mo)
Titanium (Ti) Max. 0.20 + 4x (C + N) Min. to 1.10 Max.
Aluminum (Al) Max. 0.15
Cobalt (Co) Max.
Tungsten (W)
Vanadium (V) Max.
Copper (Cu) Max.
Manganese (Mn) Max. 1.00
Niobium (Nb) plus Tantalum
Carbon (C) Max. 0.07
Nitrogen (N) Max. 0.04
Silicon (Si) Max. 1.00
Sulphur (S) Max. 0.030
Phosphorous (P) Max. 0.040
Other Elements

439 Product Range